Abstract
Tm-doped 790-nm-pumped silica fiber lasers are excellent candidates for producing emission at <1:95 μm, but achieving efficient operation at these wavelengths requires careful attention to fiber design because of the characteristic three-level reabsorption effects. We present a discussion of methods for mitigation of these effects and two high-efficiency systems that are capable of producing up to 70Wat<1:92 μm.
Original language | English |
---|---|
Pages (from-to) | 5072-5075 |
Number of pages | 4 |
Journal | Applied Optics |
Volume | 48 |
Issue number | 27 |
DOIs | |
Publication status | Published - 20 Sep 2009 |